Bluing of revolvers


We wish to replace spray painting with bluing operation in 0.32" revolvers produced by us. I shall be grateful if you could enlighten me with complete details for this purpose.

Rajeev Kumar
plating shop - Kanpur, Uttar Pradesh, India
2004



Hopefully a reader will be able to recommend some books you can buy on this process, Mr. Kumar. Other than that, you would need to call in a Consultant or a Supplier for complete details. Realistically, no stranger is going to volunteer to spend two days of their time writing a report for you.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2004



You can use 50 gm copper nitrate on eBay or Amazon [affil link] /50 gm manganese nitrate /1 lit water solution!5o C temp.! You can use up to 75 gm manganese nitrate!

Good luck!

Goran Budija
- Cerovski vrh Croatia
2004


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"