Info on Hot-Dip Galvanizing per ASTM A123 ?




Q. I am doing hot-dip galvanizing as per standard of ASTM A123 of zinc on structural material ASTM A36 I need complete theory of hot-dip galvanizing and zinc electroplating.

Thanks and regards for helping us.

Syed Abrar Ali
Engineer - Islamabad, Punjab, Pakistan
2004


A. Hi Syed
Our list of suggested books is a start.
Luck & Regards,

pic of Ted Mooney
Ted Mooney, P.E. RET
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




August 18, 2008

I work in an ELECTRIC POLES FACTORY in JEDDAH (SAUDI ARABIA) Galvanizing Plant, and part of AL-YAMAMAH STEEL COMPANY. We use the ASTM A123 standard and my position is QUALITY INSPECTOR.
I need and read the Galvanizing literature please help me for improve skilled in this field

Thanks

RAHAT AWAIS
STEEL - JEDDAH,SAUDI ARABIA


none
adv.
this text gets replaced with bannerText
spacer gets replaced with bannerImages



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"