Developing new paints that incorporate biocides




Q. Hello,

I am a graduate research assistant at the University of Cincinnati, I develop novel organic coating systems using silanes. I am studying paint systems that have biocides or microbicides such as silver incorporated in them to address the issue of microbial corrosion. I read in an article that Cu used in some marine coatings is being phased out as it is detrimental to marine life. I want to know what is a typical biocide used in marine coatings and also in steel pipes, silver is out of the question as it is toxic. Are there any environmentally-friendly organic mild biocides being used by the coatings industry?

Thanks,

Karthik Suryanarayanan
organic coatings - Cincinnati, Ohio
2004


A. Hi, Karthik. It is possible that copper-based "bottom paint" may be outlawed, I guess, but it isn't exactly being 'phased out'. As far as I can see, every single brand and style of bottom paint listed in the Boat U.S. catalog is copper-based and depends upon copper.

It is more than a conundrum to look for an 'environmentally friendly' paint that will kill every form of marine life from algae to zebra mussels--it's an oxymoron. But it sounds like organic biocides, which might stop their killing after a few years, would be better than basic metals like copper which can presumably remain toxic to marine life even decades after they've sloughed off the bottom of the boat and onto the bay floor. On the other hand, though, organotin paints (tributyltin) have been an environmental disaster. Whatever you put in the paint as a biocide should, I would think, completely lose its toxicity after some period, perhaps depending upon the proximity of two different molecules that can be depended upon to break or not remain in proximity after the paint wears off.

You have certainly picked an interesting and important field to do your development work in. Good luck!

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2004


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"