Home of the finishing HOTLINE since 1989

-----

How to patina brass



Q. I'm looking for a way to patina brass sign letters. What do you recommend?

Tyler Brown
- Alexandria, Virginia
1999


"The Colouring, Bronzing & Patination of Metals"
by Hughes & Rowe
coloring_bronzing
on Amazon
or eBay
or AbeBooks
(affil link)

A. Hello, Tyler. Although you can buy a commercial brass darkening solution on eBay or Amazon [affil link] h, there are so darned many colors & shades that, unless you just want "dark", having a good picture of what you are seeking can be important. I think the best answer just might be: borrow this book from your library, "The Colouring, Bronzing & Patination of Metals" ⇨

Good luck!

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.



"Contemporary patination"
by Ronald D. Young
contemporary_patination
on Amazon
or eBay
or AbeBooks
(affil link)

A. It depends on what color effect you're trying to get. Here's a couple formulas --

Verde: copper sulphate on eBay or Amazon [affil link] 8 parts, Ammonium Chloride 4 parts, Sodium Chloride 4 parts, Zinc Chloride 1 part, Glacial acetic acid on eBay or Amazon [affil link] 3 parts, DI Water 128 parts. This is a dip or brush on process. The coating needs to be preserved with some kind of sealer or lacquer to be stable.

Light Green: Ammonium Chloride 16 parts, Sodium Chloride 16 parts, Ammonium Hydroxide 16 parts. This formula supposedly is stable without preservative. copper sulphate can be added to darken the green color if desired.

The book mentioned in the previous letter is indeed excellent. There is also "Contemporary Patination" by Ron Young.

dave wichern
Dave Wichern
Consultant - The Bronx, New York
1999


A. Tyler - Several chemical companies have antiquing solutions available - Hubbard-Hall has Mi-Tique Patina. This is a room temp process for copper and brass.

Dan Brewer
chemical process supplier - Gurnee, Illinois
1999




Q. ADVICE ON LACQUERING OF ORNAMENTAL BRASS (AND STERLING SILVER), INCLUDING MIXTURE OF LACQUER AND THINNER AND APPLICATION METHODS INCLUDING POURING OVER SURFACES. ANY ADVICE AND RECOMMENDATIONS APPRECIATED.

THANKS,

JORY NEWMAN
- PIKESVILLE, Maryland
2003



Brass Lacquers
brass_lacquer
on Amazon
or eBay
(affil link)
May 20, 2010

A. Hi, Jory. Smoothness and consistency is important, so multiple very thin coats, sprayed or brushed, surely beats a poured coat. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.




Antiquing brass to bronze colour

Q. Hi, I have recently purchased some of John Penny cold patina solution. My goal is to turn it dark brown to a deep bronze colour. This works well but after a few days it starts to come off and a pink colour emerges. I am guessing this is the copper in the brass coming to the surface. Anybody had this happen after antiquing brass. Any ideas how to stop this happening?

Thanks

Alex

alex king
- eckington worcs uk
February 25, 2014


Sorry! Finishing.com is currently Read-Only.
A couple of people have asked if they can take it over.
We're trying to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"