Paint plugs in an e-coat system


We are currently in the process of switching to an e-coat system from our current powder coat system. The main concern right now is paint plugs. Currently silicon plugs are being used, but we worry what will happen with the e-coat and dip tank if these plugs fall out and break down. Will silicon plugs destroy our e-coat? Is there any other paint plug in the market that will not cause problems with an e-coat system? Thank you, Josh Kundert

Josh Kundert
- Bismarck, ND
1999



Plugs are available in nearly any type of plastic, and I'm sure there are satisfactory ones for this application. See the banner ad at the bottom of the page for several suppliers.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


You may use silicone that is fully cured and have no release of any kind. Consider to check with suppliers before using such masking products.

Kissak Sarajian
- Glendle, California
2001


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"