Letter 29050
Multiple colour acid etching on 304 SS
++++
Hi,
I am redesigning an intercom panel which is currently a 3mm thick
304 stainless steel panel, powder coated white, blue paint filled
acid etching, with a clear anti-graffiti coating. We are looking to
increase the number of colours from just blue, to red and blue. The
two colours are mostly separated except one area where they meet.
This meeting can be separated by a non-etched area if required. I
would appreciate guidance in the best methods to employ to achieve
this result. panel size: 200mm x 200mm quantity: approx. 50 units
details: ~ speaker, mic and button holes ~ weldstuds on rear.
In appreciation of your time,
Jareth Bone
electronics design - Brisbane, Queensland, Australia
Dear Reader, please --
- Answer or follow-up on this subject (in non-commercial
fashion).
-
- Post a new
question or inquiry on a different subject.
-
 |