Removing Stainless Steel Bluing  

++++

We weld 304 Stainless to 304 Stainless and I am looking for any help in removing the bluing from the weld area. We do not paint our product and would like to minimize the bluing. I have tried several methods. Cleaning afterwards is not practicle(large Quanitites).Is there a way to get rid of it with a backing or heat romiving product?