We plate copper bus bar in tin and in silver. I wanted know how we could plate aluminum bus bar in tin. What is the process to this.

Howard Leatherwood
Plating shop - Pearland, Texas, United States


++++

You cannot electroplate directly onto aluminum because it is so active that it forms a passive skin instantly. The normal procedure is to immersion plate zinc onto the aluminum via a zincating bath, and then proceed with copper and tin. As an alternative, Atotech offers a proprietary sequence for plating aluminum busbar called Alstan.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com