-----Restoring Comstock Castle cast iron stoves
Q. The Connecticut Trolley Museum has this beautiful Comstock-Castle Model A on display in our lobby. It would be great if someone could help us with some information so that we can prepare a sign for our visitors. Year of manufacture (even approximate) is most useful, also how this model would have been used - possibly (hopefully!) to heat trolley cars, train cars, stations, or ticket booths? Many thanks.
Museum Volunteer - Enfield, Connecticut
April 28, 2023
Comstock / Castle stoves, parts, memorabilia on eBay [affil link]
A. Wow! An art deco wood burning stove! Never saw anything even remotely similar, but art deco started in 1919, so I'd guess early 1920's for the stove.
It was surely designed for a public space like a trolley station.
I'll try reaching out to Comstock Castle and see if they have any records or comment.
Luck & Regards,

Ted Mooney, P.E. RET
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
Update Jan. 2024! Another art deco wood stove on ebay!
Comstock Castle stove 194.
[editor appended this entry to this thread which already addresses it in lieu of spawning a duplicative thread]
Q. I recently purchased a Comstock Castle 194 stove. I was wondering how hard it is to get parts for it? I would love to restore it but not if it's going to cost me an arm and a leg and half a lifetime to find the parts.
- Dixon California
February 8, 2025
⇩ Similar, related, Q&As -- oldest first ⇩
Q. I recently purchased an 1876 small cast iron stove at the flea market and want to restore it. It is a mess, rusty and the inside still is full of soot and some ashes. It has beautiful scroll work and Mascot Comstock Castle Stove Co. Quincy, ILL on the front of the stove.
It is structurally sound with no holes or broken parts. I don't know where to start. I don't want to do anything that will wear down the detail.
Thank you,
Sally S[surname deleted due to age of posting]- Parker, Colorado, USA
2002
A. Comstock-Castle is still in business. We can give you suggestions on proper restoration. Contact me & I'll advise. Nice to see a product last so long ... shameless plug :)
John SpakeComstock Castle Stove - Quincy, Illinois, USA
Hi John. Yes, it's wonderful to see you still in business! Please jump right in to these public suggestions on proper restoration of stoves!
There are hundreds of readers of this page, and taking the conversation private disenfranchises the 99% of the readers who were following along, only to be cut off from answers & resolutions. Please don't shepherd away the readers, but try to offer public help. Thanks for your understanding 🙂
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
Q. My neighbor recently acquired an old wood burning stove & we are going to try & restore it together. Would appreciate any tips about bringing out the 'gold leaf' effect. The back of stove says Comstock Castle Stove Co Quincy, Kansas City, Chicago, Minneapolis. The front of stove says 'Elite Economy' and the number 196.
Diane N [surname deleted due to age of posting]- Bandera, Texas
2003
A. As the original mfgr. we may be able to give you some guidance.
John SpakeComstock Castle Stove - Quincy, Illinois, USA
Q. I just read the post from Diane N., Bandera, Texas, concerning the Elite Economy wood burning stove and am very interested in knowing what she was able to find out since I also have a stove by the same manufacturer, the model number is different. Mine is model 192, Elite Economy. I am missing the front door, approximately 7 in. X 8 1/2 in. and a small top round plate, approximately 3 3/4 in. I would like to read any information on this if you know it.
Thanks,
- Texarkana, Texas
January 19, 2009
Q. I have an Elite 111 coal burning stove that my dad found in a railroad car several years ago ...
I would like some information about it and if possible how to go about finding some of the skirts that go on it. they are white and hook on.
- Greensboro, North Carolina
2004
by Kathryn McNerney

on Amazon or eBay
or AbeBooks
(affil link)
Q. Just got a Redwood Comstock Castle model 38 given to me. I was wondering if anyone has any information on the year this is. It is in fair shape , but in need of some TLC. Has ornate relief on exterior of stove. Any Help will be great.
Patrick F [surname deleted due to age of posting]home owner - Kingsford, Michigan
2004
A. Regarding the Redwood. It is an iron box heating stove. We made it for several decades in the mid-late 1800s. Sold a lot to the Indian Territories. Redwoods are easy to restore if the parts are not cracked.
John SpakeComstock-Castle Stove Co.- Quincy, Illinois
Thanks John!
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
Q. I recently purchased an old Aurora Comstock Castle Iron Stove at an auction. I own a 102 year old victorian home and would like to restore this stove and use it if possible. Anyone know how old this is and how to restore it? I have cleaned off most of the rust, but don't know what to do next. Help?

hobbyist - Parksley, Virginia
2004
Q. My mom bought a stove. It has to be over 50 to 60 years old and its an Economy Comstock Stove that is wood, coal and gas burning with 6 burners.

Do you have any idea how to fix it up?
homeowner - Waterbury, Connecticut USA
July 13, 2010
Q. I recently acquired a cast iron stove by Comstock-Castle at a really good price it seems to be model#348. It does have some rust and missing hinges to the doors but would like to restore it. Could start off as a nice hobby for me. Anyone have any suggestions on what to use to clean the rust and wear? Thanks.
Julia sotoHome remo. - Tucson, Arizona
March 5, 2014
Q. I have just acquired a Comstock castle wood stove model Cub Economy #113. wondering how old it is. It is in perfect condition, and I am getting ready to put it in a restored old cabin. It is missing the collar that goes to the stove pipe. Can I buy such a thing or need to have it fabricated by a fireplace shop. Grates and everything in great shape, chrome needs a little refinishing but over all what a great find. Thanks for any help
Bill Allen- Wapiti Wyoming USA
February 20, 2017
Q. I am searching for information on a Comstock Castle PRINCESS ECONOMY wood stove. Date of manufacture and any pictures of what the stove would have looked like when new?
Lover of old cast iron stoves - Saint James, Missouri
December 20, 2021
Ed. note: Please see eBay for typical cast iron wood stoves -- they have hundreds for sale 🙂
Wood Stoves
on eBay
(affil link)
Q. I'm missing a couple foot warmers and the top front trim piece for the stove. Does anyone know where I might find parts for this stove?
- Tucson Arizona
January 19, 2022
Ed. note: Can't promise anything, but if you can't find it on the eBay link just above, please see thread 10039 where we list all known sources for parts.
Ed. note:
Letter 11428, "Restoring a cast iron wood stove completely covered in rust" compares sand blasting, wire brushing, and steel wool for clean up, plus stove paint vs. stove wax as a finish.
Letter 19039, "How to restore antique cook stoves" suggests types and sources for parts.
Letter 13218, "Restoring Nickel Plating on Wood Cookstove" may be of interest if the stove includes any plating.
Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.