Seeking SIC's of Companies using Electrostatic Coating Processes


I am a semi retired professor of manufacturing technology from Bowling Green State University, I am planning a workshop to introduce industry (manufacturing) personnel to electrostatic spray coating, and I am not an expert in this field. In cooperation with a manufacturer of E. S. equipment (they will do the teaching), a 3 day program is planned for mid November. I am having a great deal of trouble identifying the SIC's of manufacturers who use E.S. paint and powder coating as a finishing process in their manufacturing operations. This problem is such that Cahners Publishers (Ind. Paint & Powder) cannot provide me with a targeted mailing list of companies such as above, nor can Harris Industrial Directory, and I have not found such a source elsewhere. I wish to contact: manufacturers who use these processes, companies who provide the custom E. S. coating services to manufacturers, and companies supplying coating products for E. S. coating, by SIC if possible. These would be the interested parties for potential participants in the workshop. I am not interested in companies who manufacture E. S. coating equipment. Does anybody know a source of SIC's or mailing lists/email lists for the company groups above? If not does anyone have any thoughts on how I might track down this information? I will be grateful for anyone's help/information.

Richard Kruppa
Bowling Green University - Bowling Green, Ohio
1999



As a local branch officer of A.E.S.F., I purchased mailing lists from Products Finishing magazine (Gardner Publications, Inc., 6915 Valley Ave., Cincinnati, Ohio 45244-3029), and they were able to sort geographically. I don't recall if they were able to sort by what processes the shops in question did.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.



Other potential sources are: National Paint and Coatings Association 202-462-6272 npca@paint.org, Powder Coating Institute 703-684-1770 Fax 703-684-1771 ( No email address given) Send inquiry to Carl Izzo and/or Nick Liberto Products Finishing www.pfonline.com/experts/ Hope this is some additional resources, good luck.

Tyrone L. Caley
- Jefferson City, Missouri
1999


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"