Need test kit to find lead paint

Q. I need portable cheap lead detectors for paint

cort stull
- mcalester ok
1999


Lead Test Swabs
lead_test_swabs
on eBay
or Amazon
(affil link)

A. There is a product called "Lead Check Swabs" made by BGI Incorporated. You should be able to find them with a search. I talked to them on the phone and they seemed very knowledgable and helpful. There are also lead testing crayons commercially available, though I have heard they're prone to give false positive readings.

dave wichern
Dave Wichern
Consultant - The Bronx, New York


A. It depends on what you mean by "cheap", and who the analysis results are for. If you need results that are going to be in any way required or reviewed by regulatory agencies for compliance, or if your customers are going to be held to account in the same way, Atomic Absorption Spectroscopy on eBay or Amazon [affil link] is the cheapest, by far.

rachel cassai
- olympia, Washington


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"