Nikasil on plastics


We're involved in a project which needs to electroform a thick Nikasil shell (2-3 mm) on plastics (ABS). We can provide metallized parts but need help for Nikasil plating. If you happen to know the companies which can provide this kind of services, especially in Canada or USA, please say. We would appreciate your help very much. Best regards! Ke

Ke Zhang
Queen's Uni. - Kingston, Ontario, Canada
1999

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).



ke, we are doing electroplating on abs. please inform what is "nikasil". is it nickel sulphamate? thank you, daniel

daniel livshitz
- tel aviv israel
1999



Gentlemen, please start with letter #1671 which will answer your questions, and includes further links to other letters on related subjects. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"