Info on Cobalt-Zinc or Cobalt-Nickel alloy plating

1999

Hi.. I am after information on zinc-cobalt and zinc-nickel plating, a 'new' process that my employer has shown an interest in. Since I am new to this firm, I would love to be able to further cement my position in the company by being able to show him plenty of information on the process - plant needs, chemicals, etc. If all goes well, I may get one thing I've wanted since joining this firm - my own plating plant to play with :-)

If the info is to large to publish here, could you please provide me with links to suitable sites, or e-mail me the info. Am also interested in just making contact and chatting with other platers.

Thanks in advance and thanks to finishing.com

David Chord
plating shop - Porirua, New Zealand



1999

The Zinc alloys plated with either iron, cobalt, or Nickel are viable alternatives to cadmium plating. New techniques are being devised all the time. The zinc/nickel will give the highest degree of protection to salt fog, while the zinc/cobalt will offer better Kesternich (sulfur dioxide) Test results. Zinc Cobalt may be plated out of either acid or alkaline baths. Zinc Nickel gives best results from an alkaline non cyanide bath, and is offered in two types.
1. Low Nickel= Plates 5 - 9% Nickel in the alloy.
2. High Nickel = plates 10 - 15% Nickel in the alloy.

The European community favors the High Nickel, while the far East and U.S. markets now favor low nickel.

ed budman eb sig
Ed Budman [dec]
- Pennsylvania
With deep sadness we advise that our good friend Ed passed away Nov. 24, 2018



Hi

I am looking forward to have information on Cobalt - Zinc alloy plating. I would like to know about some information on what exactly the process is? What I am looking for is its application on aluminum base? Can you suggest me any book or research paper? Awaiting for your reply.

Thank You,

Bharat Panchal
- Cleveland, Ohio
2002


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"