Letter 28024

How to place the fasteners and shafts in salt spray test chamber [India] 

++++

Hello,

Painted panels can be hanged in test chamber but I would like know the standard practices of positioning the fasteners & motor shafts in the salt spray test chamber?

Prasanna N.
Q.A. - Aurangabad, Maharastra, India


++++

SAE/USCAR-1 requires that the orientation of the primary axis of the fastener to be 25 +/- 3 degrees from vertical. I recommend that you obtain this standard, as it describes the proper procedure for testing fasteners, and it is suitable for shaft components as well.

Toby Padfield
Automotive module supplier - MI, USA


++++

Painted panels should be tested at a 15 - 30 degree angle. For other parts, the significant surface should be a 15 - 30 degree angle whenever possible. Position the test specimen to minimize solution collection in crevices.

Cynthia L., Meade
National Exposure Testing - Sylvania, OH


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com