Alternatives for ni-cr plating of brass [North Carolina] 

++++

We are looking for alternatives to Nickel/Chrome over brass that is aesthetic as well as durable. We are open to all suggestions. One of the components is a brass ferrule that will be crimped and the finish must adhere after this process. This component is .850 ID with a wall thickness of .025 and the length is .625 with a hole pierce of .550. We would like the finish to be a yellow color. The other component is approximately 2.250 L x 13/16 W. This has internal threads at 1 end and a 1 piece stem on the other to be crimped on hose. Again this must withstand crimping. We are currently using a commercial Zinc plate for this. The finish needs to resemble the clear Zinc yet provide better resistance to the elements. As is always the case we are looking to beef up both without the added cost. Total yearly volume could exceed 500,000 pcs.

Mack McPeeters
fire protection industry - Greensboro, North Carolina, USA


++++

Electroless Nickel.

Todd Osmolski
Charlotte Plating, Inc.

Charlotte, NC USA


++++

How about electro-catalytic nickel. It has almost no stress, good corrosion resistance, great appearance, and less cost than electroless. Happy to do some samples for you.

Dan Weaver
Team Metal Finishing - Toccoa, GA


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com