I have installed a gas effect fire with a chrome surround. Whilst treating a lintel above the fire with a paprika dye, some staining has occurred on the chrome which won't come off with a soapy cloth. Are there any cleaning products I can safely use?

Mary Holding
hobbyist - Sheffield, South Yorkshire, United Kingdom


+++

Chrome is quite abrasion resistant. If it's real chrome you can use abrasive cleansing powder like Bon-Ami [link is to product info at Amazon] or even Steel Wool [link is to product info at Rockler] judiciously. But it may not be chrome. So see if there is a plated area which is not visible that you can test these approaches on.

 
Ted Mooney, P.E.
finishing.com Inc. - Brick, NJ


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com