Letter 26677
Nickel plating
[Texas]
++++
I work on cash registers and barber chair. I would like
to know how to nickel some items. Do you have a nickel
plating kit, or any advise.
Thanks,
Victor Sepulveda
I restore antiques for my use. - Natalita, TX, USA
++++
For your use, consider "brush plating". Check out the
vendor lists at this site. This procedure is extremely
operator sensitive. If you want a lot less pain, attend the
free school from the folks that you think that you want to
buy the equipment and solutions from. Typical is 3-5 days of
lecture and hands on. Good equipment makes a huge amount of
difference, so look at more than one vendor.
James Watts
- FL
----