The right maskant.


1999

Several Years ago we purchased a green colored plating maskant manufactured by a company called "Turco". The carrier for the maskant (VOC) is perchlorethylene. When we ran out, we found our distributor was no longer in business and could not find the manufacturer either. None of the other maskants we have tried since will properley do the job, in fact our reject rate has quadrupled! The job itself is a .00035" thick nickel electroform from an aluminum mandrel which must be washed out in caustic soda ⇦liquid caustic soda in bulk on Amazon [affil link] . Does anybody know the whereabouts of Turco or of a perchlor based maskant? Help please.

Anthony J. Covey
electroformer - Corona, California


Nolan maskant Producer: Schramm Germany

Piotr Lobodziec
- Warsaw Poland
1999


In response to Anthony J Covey's question, Turco Products is in Long Beach, CA.

Mike Fox
- Seattle, Washington
1999


AC Products, Inc. manufactures a product similar to the Turco product which is solvated in perchloroethylene.

Sheldon Weinstein
AC Products, Inc. - Placentia, California
2000


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"