How to coat nitrided parts for 600-hour salt spray resistance

Q. Hi, We are looking for any product which can protect nitrided steel parts against 600 hour salt spray test. Thank you for your earliest answers.

P.Bourdareau
surface techniques - Andrezieux Boutheon, France
1999


A. You coat the teflon/xylan/dyflon/greblon/rilson corrosion-resistant fluoropolymer coatings.

kalyan dhakane
Kalyan Dhakane
Mumbai, India
2000




Q. I am interested in attending a seminar to learn more about the nitriding process. Is anyone aware of a nitriding class/seminar?

Thanks,

Valerie Jennings
- Gastonia, North Carolina
2001


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"