I have read the FAQ's and did not see this question. We have a
situation where the green corrosion from copper pipes has dripped on
the carpet. I am looking for the best way to remove this material.
This will be performed by a professional carpet cleaner.
Thank you in advance,
Bill Yeadon
cleaning - Westerville, Ohio, USA
These copper salts should readily dissolve in even mild acids. I'd
suggest trying white vinegar followed by soapy water. Good luck

Ted Mooney, P.E.
finishing.com Inc. - Brick,
NJ