Tungsten carbide inserts get brown patches from cleaning [India] 

+++

We are facing problems in cleaning of tungsten carbide inserts. The inserts are getting brown patches on ce we dry the inserts after cleaning. The process is as follows.

1. Tank 1 - Acidic medium,60deg Cel,with ultrasonics,30 sec
2. Tank 2 - Demin water,60 deg Cel, with ultrasonics,30 sec
3. Tank 3 - Demin water,60 deg Cel, w/o ultrasonics,30 sec
4. Tank 4 - Demin water,60 deg Cel, with ultrasonics,30 sec
5. Tank 5 - Demin water,60 deg Cel, w/o ultrasonics,30 sec
6. Tank 6 - Demin water,60 deg Cel, with ultrasonics,30 sec

w/o - without.

Note: Tanks 1,2,3 and 5 have circulation system with filters of 25,10,5 and 3 microns respectively. Could you kindly throw us light on the problem.

Mr. Ravishankar. S
Asst. Manager - Production Engineering - Bangalore, , Karnataka, INDIA


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com