Hard chrome wear off and replating
[India]
+++
We tried Hard Chrome coating of around 20-30 microns on HcHCr tool
steel with hardness of 54 Rc. It showed good results and the
dimensional change was within our requirement.
The objective is to closely maintain the dimensions.Now as the
hard chrome wears off the entire tool must be stripped and rechrome
plated "JUST BEFORE" the previous coating has worn off at any
region.This will preserve the dimensions of base substrate. Is there
any simple (non-destructive) way to determine the regions where the
chrome is worn off or too thin to serve any purpose.
Thanks,
Gaurav Garg
Manufacturing - New Delhi, New Delhi, India
Dear Reader: please choose what you want to do--
- I want to answer or follow-up on this subject
publicly (in non-commercial
fashion).
-
- My company is a supporting advertiser at
finishing.com and we want the contact information to reach
the inquirer privately.
-
- I want to post a new
question or inquiry of my own on
a different subject.
-
 |