Speed of deposition in brass bath  

+++

Which are the conditions of work of a brass bath to get a good speed of deposition in brass bath high layer?

Diogo Cavalcanti
Home Hardware - Caxias do Sul, RS, Brasil


+++

Hi. The single thing that must be done to increase the speed, according to Faraday's Law, is to increase the current density. But how to achieve this, while avoiding consequent problems like burning, is difficult to discuss in the abstract. Are you using a cyanide or non-cyanide brass plating bath, Diogo?

You might be interested in Brenner's "Electrodeposition of Alloys".

 
Ted Mooney, P.E.
finishing.com Inc. - Brick, NJ


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com