finishing.com -- The Home Page of the Finishing Industry Search our quarter-million Q&As

Home of the finishing HOTLINE since 1989

-----

PEO on aluminum





Q. Hello:

I am a university student. I am searching some information about a method to protect aluminium named PEO (Plasma Electrolytic Oxidation). If there is any help available, it will be gratefully appreciated.

Thanks.

seckin tohumcu
student - bursa, turkey
2003



April 2, 2009

A. Hi,
PEO means plasma electrolytic oxidation.
This process is applied on light metals like aluminium, titanium, magnesium, ...
This process needs a nice power supply with min. 600 volt output in bipolar and constant current mode.
This process has 2 issues:
1- electronics hardware (how to apply voltage and current applied) that are needed.
2- electrolytic chemicals

behrouz asli
- tehran, iran


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"