I have an antique Moroccan brass table which is heavily tarnished (green build-up). It does not have a finish on it. I have tried brass polishes, but obviously they don't get rid of the green tarnish/build-up. I greatly appreciate any suggestions on restoring the brass.
Carla JohnsonStudent - Blacksburg, Virginia
2003
Hi, Carla. Although easy on people, vinegar
[in bulk on
eBay or
Amazon] plus salt is very aggressive on brass. Some people add flour to give it a bit of grit for polishing. If there is fine detail on the table, be careful because the stuff is aggressive. It will leave the brass the brass raw and orange, but that can be mellowed out with the brass polishes you already have on hand.
Please see letters 9922 and
22177 for more detail.
Regards,
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
October 20, 2009