I want to get a set of chrome rims dipped. Where can i go?
Kevin W
Mertiage - Va Beach, Virginia

September 23, 2009
Hi, Kevin. The banner at the top of the page leads to plating
shops which specialize in restoration of automobile parts, or you can
use our Jobshops Directory to
locate plating shops in specific areas or which do specific
processes.
Unfortunately, if these are aluminum alloy wheels, you may find
the restoration cost unacceptable. It's a complicated process and the
old issue of labor cost is a killer. We have an
Introduction to Chrome Plating on
line if the subject really interests you, as opposed to just getting
the job done :-)
New wheels are processed dozens at a time in automatic plating
lines whereas restoration involves fighting with the details of each
particular wheel one at a time. Frankly, you will probably find that
replating costs more than new wheels and, unless they are really
special or of sentimental value, not worth it. But best of luck
either way!