SIMPLIFIED PRETREATMENT FOR POWDER COATING

   

+++

I'M USING THE SEVEN CHEMICALS TO CLEAN THE MATERIALS BEFORE COATING THEM.
I WANT TO KNOW IS THERE ANY NEW CHEMICAL FOUND THROUGH WHICH I CAN INCREASE THE PRODUCTIVITY AND ALSO REDUCE TIME AND ALSO INCREASE QUALITY.

THANK YOU VERY MUCH

DILIP ISHWARBHAI PANCHAL
POWDER COATING - BARODA, GUJARAT, INDIA


+++

Dear Mr. Panchal,

If you are using the seven stage pretreatment, we presume you are using zinc phosphating. Now, if your component contains rust, then this method is necessary.

In case the components are without rust, and the customer does not have a requirement for zinc phosphating, then there are single stage, no-rinse single tank pretreatments in the US and Europe which can do pretreatment in one stage.

However, they have not taken off well in India, primarily due to rust problem.

Regards,

Sandeep Kundra
manufacturers of metal pretreatment chemicals - Bombay, Maharashtra, India


++++

Where can I find out more about these one step pretreatments that are used in Europe for rust free mild steel?

Jerry Jaksha
- Rio Rancho, New Mexico


October 17, 2009

Hi, Jerry. All of the manufacturers of pretreatment chemicals, like Chemetall, have one-step pretreatments in their repertoire.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search