Masking for chrome


1999

I am looking for a masking application for using in a chrome solution. I like to use lacquer for masking before I put the part in the chrome solution.

Sincerely

Anders Sundman
Anders Sundman
4th Generation Surface Engineering
Consultant - Arvika,
Sweden



In the USA, there are several companies that make the lacquer you refer to, and numerous firms that sell it or repack and sell. You should have several choices in Europe. It probably will take one more coat than they reccomend for heavy build ups.

James Watts
- Navarre, Florida
1999



Lacquer is the most time consuming waste of a chrome platers time . There are many other ways of protecting surfaces . I stopped using lacquer years ago , and found it much faster to develop new methods .

Dave Brackenridge
aerospace plating - Germiston, South Africa
1999


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"