Why is the color of our silver plating constantly shifting?




1998

Dear Sir,

Can anyone please explain to me the cause of hue difference in Ag plating process? I realized that this hue difference often occurs on when the plating area is large (die pad area of IC leadframe). Does this hue difference occur when the current density drop? How can I overcome this problem.

I look forward to your reply.

Thank you!

Alex Yap Chee Wai
Hitachi Cable Singapore


Dear all,

In Ag plating process, I meet a question . During plating Ag, the substrate material--Cu is not its own colour and the thickness of Ag in die pad in the lead frame the is not even. If you know ,please help me ! If you are working in the plating about the leadframe ,I would like to make friends with you !

Best Regards!

Wung Feng
QPL - Shenzhen, China
2002


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"