-----Pump problems with palladium-nickel rinses
1998
Hi-
I have a question regarding Pd-Ni Rinse waters and the types of pumps to use with them. We have had recurrent problems with pumps used to transfer these rinses. We have experienced seal and impellor failures and it appears now that our mag pump has failed, the exact mechanism still to be identified. Does anyone have experience with this situation who could offer me some advice?
Thanks in advance.
JDK
JD KroniczI'm just wondering what pumps you are using and at what flow rates?
Larry Genest1998