Letter 24059

Paint is peeling off  

+++

My company having serious paint peel off problem for regal grey parts. Some parts produce blistering before peel off. What are the areas that we can study to overcome this problem. pls advise me. 2) we are doing cleaning processes like degreasing, water rinsing and pickling. this degreasing process actually creates a lot of foam. we are facing to difficulties to clean this foam. any idea. pls advise me.

Murugan s/o Rasamanie
spray painting company - Kuala Lumpur, Selangor, Malaysia


+++++++

Normally to avoid the foam the water should be at 50 deg C if is cooler you will have foam.

Eduardo Carrillo Contreras
- Cd. Juarez Chihuahua, Mexico


Dear reader

Post an answer
 
Post a question
 
Report broken links

 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com