Removing lime deposits from chrome bathroom fixtures

+++

I have what appear to be lime deposits on my chrome bathroom fixtures (faucets, towel racks, etc.) and am wondering what is the best and most economical way to clean them and remove the deposits and spots.

Mae Cheung
- South Bend, IN, USA


+++

There are readily available products like CLR [link is to product info at Amazon] , designed for removing calcium-lime deposits.

However, some bathroom fixtures are plated zinc diecastings which, after their useful life (which may be only a few months if they are low quality), 'bloom' with white pits and pimples. I would be surprised to see calcium deposits building up on towel racks, so I fear this may be the case. But get some CLR or equivalent and try it.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com