Letter 23765

Removing oil stains from diecastings [Phillippines] 

+++

I'm working on a die cast company.We use aluminum ADC12 material for casting.One of our problem is stain occuring after casting that we use to recover the product by folishing after blasting.
I would like to ask advise, what chemical will be better to apply to eliminate the stain on the surface of the product or any other alternatives to eliminate stain.
By the way,this stain is cause by oil and lubricant during die casting.

Jerson Sanchez
product engineering - Cebu City, Cebu, Phillippines


Dear Reader, please --
Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com