Project Report for setting up Powder Coating unit



Q. We plan to start a powder coating unit. Looking for project reports detailed to include machinery, market condition, source of funds, manpower requirements, etc.

Mohammed [last name deleted for privacy by Editor]
- Navi Mumbai, Maharashtra, INDIA
2003




Q. I want to start a powder coating business in Palwal.

Sarjeet Singh
powder coating - palwal, haryana, India
April 4, 2016



A. Hi Sarjeet. You can get some introductory info right on this website, with our library articles "Introduction to Powder Coating" by Mario Pennisi, "Cleaning & Rinsing for Powder Coating" by Bob Utech.

"User's Guide to Powder Coating"
by Nicolas Liberto

on Amazon
or AbeBooks
(affil link)

Then you might to consult the Metal Finishing Guidebook although it is no longer published.

After that, they are many excellent powder coating books.
If you have a specific question, I think our readers will be able to help!

Regards,

ted_yosem
Ted Mooney, P.E. RET
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
April 2016


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"