Nitrotec Surface Treatment Information Request


Nitrotec surface treatment: I need some help on defining a process specified by a new customer. The customer has specified the Nitrotec-S surface treatment, I know that this process is a licensed process with minimal licensees in the USA. However there are similar process that claim to produce like results in surface finish, corrosion resistance, lubricity, & black color. IE.NU-TRIDE, Lindure, etc. Is Ferritic Nitrocarburizing the generic name for the similar processes and is there a standard process? Any information on this process will be greatly appreciated.

Mike Colasanti
- Kalamazoo, Michigan, USA
2003



2003

The Nitrotec process is actually a Gas Nitriding process, not a Liquid Nitriding process. Liquid Nitriding can be further subdivided into cyanide bath processes or non-cyanide bath processes. Ferritic Nitrocarburizing can be performed in either liquid, gaseous, or plasma environments, but is probably most associated with liquid processes carried out in non-cyanide baths.

There are a number of industry standards that cover these types of processes, and really should form the basis of a drawing specification, not the use of trademarks or tradenames for the various patented and licensed processes. The following list references the various standards and tradenames:

SAE AMS2759/6 & SAE AMS2759/10 - Gas Nitriding standards (Nitrotec)
[Ed. note Jan 2011: AMS2759/6 was replaced by AMS2759, AMS2759/10 is now withdrawn]

MIL-STD-1876 - Gas Nitriding (spec has been canceled)

SAE AMS2753 - Liquid Salt Bath Ferritic Nitrocarburizing (non-cyanide, NUTRIDE, ARCOR, MELONITE)

SAE AMS2755 - Molten Salt Bath Nitriding (cyanide-based, TUFFTRIDE)

Lindure is a gaseous ferritic nitrocarburizing process from Bodycote, but I believe the process standard to which it meets has been canceled (SAE AMS2757). It is possible that SAE AMSS6090 Steel Carburizing and Nitriding, Processes For is a general standard that covers this process, and the others as well. I would recommend using one of these standards as the basis for specifying product characteristics and requirements.

Toby Padfield
- Troy, Michigan



Nitrotec-S is more than just gaseous ferritic nitrocarburizing. It includes at least one specified post treatment and may include others not identified. There are three licensees in the US. The process used to be covered by up to 8 patents in the US and I think that there is one or two remaining. One patent covers Nitrotec-S (#4,881,983) and therefore can not be duplicated without violation of the patent or disappointing the customer, or both.

Arvid Casler
- Cherry Valley, Illinois, USA
2006



December 14, 2012

Thanks for the warning, Arvid... maybe Mike can get the spec changed. Most professionals are highly in favor of companies offering proprietary processes, and either patenting them or keeping them as trade secrets, and exercising good stewardship over them; but are generally opposed to seeing brand names written into specs.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Which gasses are required for this process and what's their functions?

Ravi Kumar J R Javagal
hightemp furnaces - Bangalore
September 29, 2008



January 10, 2011

hello sir,
i have a little knowledge on Nitrotec treatment, that it is a surface engineering to enhance the properties like Corrosion and wear resistant surface High surface hardness etc, but my question is related to its inner hardness, and does Nitrotec heat treatment enhance machining properties, please let me know about this.

Thanks

MANTESH.C CHOUKIMATH
student - Bangalore,KARNATAKA, India



Hello I'm a material expert and I need some help about Nitrotec NQ40 and Oxynitrocarburation technology. What is the NQ40 material? Could you explain this process ? Can I substitute other process for them? How can I do it? I promise you can help me.


Mohammad Zarghami
Sapco - Tehran, irankhodro, Iran
2003



2005

Dear Mohammad,

You can contact the company:

Mamasta
Spikweien 27
5943 AC Lomm
Netherland

Best Regards

Heinz Westerhoff
- Germany


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"