Hard anodic coating on magnesium alloys

none
adv.
this text gets replaced with bannerText
spacer gets replaced with bannerImages


Q. I would like information on hard anodising process for Mg alloys. Is it a most usual process dangerous? There is a special one based on micro arcing (plasma chemistry anodising)? Can any one tell me more about this?

Thanks,

Anibal Portinha
- Braga, Portugal
2003


A. There are a number of companies that have developed anodic coatings for magnesium using conventional and newer micro-arc oxidation processes. For general information, try:

Anomag
Tagnite
Keronite

For more technical information, go to Metalast, then click on The Technology, then Research, then Technical Bulletins, and then either Micro Arc Oxidation or Mg Anodizing.

Another great place to obtain detailed technical information is from the patents of these various coatings. You can access US patents free-of-charge from the US Patent Office website http://www.uspto.gov/

European and other patents can be obtained from the European Patent Office website http://ep.espacenet.com/

Toby Padfield
- Troy, Michigan


Ed. note: You may also want to contact some shops which do anodizing of magnesium, as listed in the banner at the top of the page.




Multiple threads merged: please forgive chronology errors and repetition  🙂



Magnesium coatings pretreatment

Q. Dear reader I am interested in coating of Mg alloys by epoxy, but as you know pretreatment is very important, so will you tell me how permanganate or other pretreatments can be done to enhance the adhesion. Issa

issa M. Baghni
Education - Beijing, China
2003


A. Check out the FAQ on Mg finishing. FYI, the DOW anodizing treatments are quite porous, and not as good as the newer generation coatings like Tagnite or Anomag. Norsk Hydro has published some work on the use of permanganate pretreatments as replacements for chromates, including an article in the October 1995 issue of Metal Finishing. Henkel Surface Technologies has an Alodine product specifically developed for magnesium.

Toby Padfield
- Michigan




Corrosion resistant coating for magnesium

Q. Dear all, we are producing small medical devices (a kind of wire netting) made of a special magnesium alloy. To archive further corrosion resistance we want to finish the surface. The use of elements which are potential allergenic (e.g. Ni) is inappropriate. The best would be a kind of magnesium oxide coating. Which could be a suitable process to achieve a graduated corrosion stability?

Thanx!

Eric Wittchow
Research scientist - Erlangen, Baveria, Germany
2004


A. I have not seen any product made of magnesium that I like except for a camping tool that you scrape off the surface and emit sparks on it to start a camp fire magnesium deteriorates so rapidly compared to most metals, you could try a really fine coating, maybe bronze, but I would recommend looking for a replacement for the magnesium!

Stephen Duvall
oilfield services - Elreno, Oklahoma


A. Magoxid-Coat(r) is a patented, hard anodic coating for magnesium. It is very corrosion and wear resistant.

Chris Jurey, Past-President IHAA
Luke Engineering & Mfg. Co. Inc.
supporting advertiser
Wadsworth, Ohio
luke banner


A. I agree that you should investigate magnesium oxide coatings produced by anodic treatments. Luke Engineering & Mfg. Co., Inc [a finishing.com supporting advertiser] MAGOXID-COAT and MAGPASS-COAT may be suitable. Other coatings like Keronite (UK), Tagnite (US), and Anomag (NZ, USA) are available as well.

Toby Padfield
Automotive module supplier - Michigan




Q. What is ANOMAG Anodizing? Does anyone know the process of it ?

Asrith Puttaganti
- Vijayawada, AP, India
June 11, 2014


A. Hi Asrith.

Hopefully the thread we attached your inquiry to will give you a good start. Best of luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.



Q. Can you tell me whether we can use Anomag for Aluminium alloys ?

Asrith Puttaganti [returning]
- Vijayawada, India
June 18, 2014


A. Hi again, Asrith. Anomag is a proprietary process for anodizing of magnesium, so it's hard to learn much about it without being a licensee, and I'm not.

I'm not quite sure what it really means when you are interested in applying a magnesium coating process to aluminum, because while you could perhaps get good quality aluminum anodizing in the same tank used for magnesium (maybe) by re-adjusting every parameter, as soon as you are not processing magnesium, you are not doing Anomag. So what do you really mean?

I would suggest contacting IHC (International Hardcoat) [a finishing.com supporting advertiser] , as they are both an Anomag licensee and a hardcoat aluminum anodizing shop, and they can doubtless answer your questions if they can clearly understand it. Best of luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"