Q. Just started work as EH&S; coordinator at a company with a new powder coating operation. Unfortunately no one seems to be aware of environmental or safety issues with powder coating operations. Are there any websites that provide insights on these issues? Thanks for any advice!
Bonnie P [surname deleted for privacy by Editor]- Cincinnati, Ohio USA
2000
Q. I am looking for a source or suggestions of employee Safety Recommendations when using powder coat systems.
Paul R [surname deleted for privacy by Editor due to age of posting]A. Actually, you came to the right place.
Thread 13877 talks about NFPA requirements for the booth and installation area. For other issues ask a specific question, and you are liable to get an answer.
For instance, ;-)
We handle waste powder from the coating operation by sweeping it up into a paper bag, then collecting the bags in the furnace room. Is this a good idea? ;-) Tom
Tom Pullizzi
Falls Township, Pennsylvania
2000
A. For a general introduction to the issues, CCAI (CCAIweb.com) offers a 225 page "Hazard Communication Pocket Handbook" which is pretty good, and at $8 (even less for CCAI members) plus $5 shipping it is quite the buy!

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
Hoods for powder coating
Q. I am a PCD applicator (painter) for a commercial lawn mower mfg. company. We are having safety issues on whether or not our PPE is safe. For instance, one painter has what we call a leather outer shroud, this goes around the bottom of our helmets and tucks inside of our suits. It is the only one in the plant. The safety coordinator is saying that the paint is seeping through the leather. The rest of us have a plastic shroud. and they leak just as much if not more paint than the leather one. My question is, is the leather one any better? Is it unsafe? Are there any other form of shrouds out there that would do the job of keeping a powder paint out better than the leather or plastic ones we now have? I hope this is enough information, if it is not, please ask what else you need to know, I will do my best to tell you what you need.
Thanks for your time,
comercial lawn mower mfg. - Fairbury, Nebraska, USA
2003
A. My first question would be whether either or both of the shrouds have approval ratings from standards authorities. Do they claim to meet any ANSI standards?

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
Q. Ted,
I have done some checking about the outer shrouds and have only found information on the plastic one so far. I do not see anywhere on the package that it says it is ANSI approved or meets ANSI standards. It does say however that it uses are, General Purpose W-5005, Abrasive Blasting W-5006, and Welding W-5003. Unless Powder Coating is considered General Purpose use, I don't see anywhere on here that it is for powder coating. As I said before, the paint does go through the cracks in the seems, therefor it is not completely sealed. As for the leather ones, I have been told that they are for welding, but seeing that the plastic ones are also, I can't see the difference or harm in using the leather one. I would greatly appreciate you help on this subject, if you are able. I thank you for your time and hope I have given you enough information.
Thanks again,
commercial lawn mower mfg. - Fairbury, Nebraska, USA
A. Hi, Lacey. Those numbers seem to be 3M codes for general purpose, abrasive blasting, and welding helmets. If you can't find any specific requirements for powder coating helmets, I'd say the W-5005 would be right helmet, and that your plastic shrouds, which 3M apparently includes or lists for this helmet, are the best choice. But 3M has an "R-Series Air Crown Headgear" suggested for powder coating, so they may be able to explain any differences between this and what you are using, and why it might be better.
It's possible that the leather shroud is an older 3M accessory for the same helmet, but who knows? Sometimes we are forced to throw out leather shrouds and old world wooden cutting boards (as the New York City chefs were ordered to do) before we find out that the plastic ones are more dangerous than what they legislated to throw out after all 🙂
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
Is a mask required for powder coating?
Q. What type respirator is the best to use on a powder coat line?
Mike S [surname deleted for privacy by Editor]- Leola, Pennsylvania, USA
2003
Q. I been working as a painter for several months. I deal with powder coating every day with no mask. I get paid less than $9 an hour. There ain't no hazardous signs up anywhere. Well my first question is: is it dangerous for my health to work without a mask? Second question is how much does a painter dealing with powder coating gun get paid?
Richard [surname deleted for privacy by Editor]- Texas, united states
October 13, 2012
A. Hi Mike, Hi Richard.
I'm not sure that there is a need for signage as it's quite possible that no toxic or hazardous materials are involved. But you should not be inhaling anything. If you are spraying within a booth, I would think you should have a proper respirator. If you are outside of a tunnel, operating something remotely, I don't know whether you would need to wear anything. You can anonymously call an OSHA Hotline and your workplace will be inspected.
Richard: You are apparently in a non-union position in a non-union shop, so there isn't any standard wage. But I would think that if you've applied yourself over the last several months so that you've learned something, you should be able to land a position with a reputable firm that cares for their employees safety and pays a prevailing wage. Remember that if you work for a bad outfit, you're helping them undercut legitimate shops and win contracts, which pulls down everyone -- so you are not just a victim, you are part of the problem. See if you can't find a better position. Best of luck.
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
PPE for Operators of Powder Coating Systems
Q. What is the right "PPE" Personal protective equipment for operators while doing powder painting? I need the info or the website address.
Nanda Srikakulamelevators - Bangalore, India
2001
A. All powder coatings (and any other chemicals/products) that you purchase should have corresponding MSDS sheets with them. The MSDS sheets have a section which tells you what PPE to wear when using that particular product.

Marc Green
anodizer - Boise, Idaho
What type of Shoes should powder coating operators wear?
Q. I need info on what type of shoes the operators should wear in the powdercoating booth. This is electrostatic operation. What should the soles be made of?
Margaret A. ReevesB&W Custom Truck Beds, Inc - Humboldt, Kansas, USA
2003
A. Any good rubber soled work boot or shoe should be acceptable. Have them wear Tyvek booties in the paint area and booth to eliminate the possibility of your tech's tracking oil and dirt from other areas of the plant into the application area. Respirators and ear plugs are generally the most important PPE's associated with the application of powder coatings. Ear plugs being most important due to high decibel's of booth exhaust fan's. Also, properly ground equipment and make sure your UV flame detection equipment is clean.
Andy PealAutomotive Components - Grand Rapids, Michigan, USA
2003
Personal protection from Powder Coating flames
Q. How do you protect painters from the flames involved in the powder coat painting process? Face, clothing, etc.?
Chuck Wade- Mattoon, Illinois USA
April 15, 2014
A. Hi Chuck. What flames are those? Either I am misunderstanding something about powder coating or you are. There is a "cure oven" and sometimes a drying oven or preheating oven, but no open flames that I know of.
The powder is sprayed on as a fine powder, sticks to the part due to static electricity, and then is baked so it flows together into a coating.
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
Q. Ted, After talking with my painter, he informed me that after the cabinet is heated, the center of the torch blows the polycoat onto the cabinet. Then after, he sprays on the powder coat with the gun and heats it back up with the torch. He says he has done it your way before, but this is much more efficient. He has been doing this for 12 years. My original question was how to protect the painter from the flames?
Thank you,
EHS Coordinator - Mattoon, Illinois USA
Hi again Chuck. As someone who has never personally powder coated anything, I'm certainly not going to claim that I know more than your operator who has been doing it for 12 years 🙂
All I can say is that I've never seen such a thing, so we'll have to wait for someone who has. Unfortunately I can't suggest a reasonable safety protocol under this circumstance.
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
A. I assume that you are talking Thermoplastic Powdercoating?
As 99.9% of Powdercoat is thermoset then that has created the confusion.
Perhaps if you could explain your Thermoplastic procedure in detail we may be better able to assist.
Are you using a Xiom System or maybe a Plascoat system?
Please advise.
Regards,
Bill
Trainer - Newcastle NSW Australia
Thanks for your insight, William. I've only seen thermoplastic powders applied from a fluidized bed, never a spray, so it's unfamiliar to me.
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
A. It is possible to powdercoat using a gar torch to heat the object then spray powder at it. This is a very crude method, and not advised. A bit like painting liquid paint using a rag instead of a brush?
There's also the flame sprayed system such as Bill mentions, Xiom (and others), where an oxy-propane gun has powder delivered by compressed air to the hand held gun such that a flame and powder are sprayed simultaneously (we have one of these).
It's controlled by a trigger on the gun, so the operator is in full control of both the gun running and the direction s/he points it. Its more suitable to thermoplastics, but can be used for thermoset powders too. The control is nothing like what can be achieved using traditional method.
It's a one handed operation. It's not necessary to protect that one hand holding the gun, which isn't hot, but it's advisable; but a simple leather glove is enough.
In this situation, safety glasses would be another way to reduce risk, but there isn't a specific eye risk.
The biggest risk is to observers, they should be kept clear.

Geoff Crowley
Crithwood Ltd.
Westfield, Scotland, UK
May 1, 2014
A. Well, it is obviously impossible to achieve a true powdercoat specification of any kind using thermo-set powders in this way.
It might be possible to produce a glossy short lived coloration, but that is all.
It simply does not have the control necessary to cross-link the polymers and achieve a true Powdercoated finish.
On the other hand if we are dealing with Thermo-Plastic powders then all that is required is to melt them, so a real result might be achieved.
Whilst I have a great deal of respect for Geoff's expertise, I would suggest that a suitable Respirator is definitely required together with eye protection and a hand protection which is Conductive.
Hope this helps.
Regards,
Bill
Trainer - Newcastle NSW Australia
"Well, it is obviously impossible to achieve a true powdercoat specification of any kind using thermo-set powders in this way."
... which is why our unit is not in use and has been in storage for some years now.
The call for thermoplastics in our market is much smaller, and we have far better control using a standard curing oven.

Geoff Crowley
Crithwood Ltd.
Westfield, Scotland, UK
I think you pretty much answered my question. Thanks for all your help.
- Matton, Illinois
"Well, it is obviously impossible to achieve a true powdercoat specification of any kind using thermo-set powders in this way."
... which is why our unit is not in use and has been in storage for some years now.
The call for thermoplastics in our market is much smaller, and we have far better control using a standard curing oven.

Geoff Crowley
Crithwood Ltd.
Westfield, Scotland, UK
Q. Hello I was curious if anyone could tell me a good kind of suit to wear while powder coat painting that will keep the powder off of your body?
Michael Terry- Hillsdale Michigan usa
December 12, 2015
Q. What type of safety clothing should the powder coating painter should be wearing? Because one of my painters has reported he has skin problems. As of now he wears casual clothing to work.
P.S. We are a small and new company.
- Dubai, UAE
September 11, 2016
Q. What is the proper OSHA PPE for the application of powder coating? Does the entire face need covering? Will a disposable particulate mask suffice? Is eye protection required? What is the breakdown head to toe? I'm writing a manual for proper PPE specific to my workplace. It's a three filter powder booth system across from the operator as metal passes between.
Mark McWeeney- Oakville, Connecticut, USA
January 7, 2017
A. Well, the answer in brief is no, a paper mask is not adequate PPE for a powder applicator.
Powder can affect every orifice and even the skin to various degrees.
The first thing is to limit exposure:
Ensure the gun earth cable is attached to the target area (usually the booth).
Ensure that the applicator is as removed as possible from the spray zone. This may mean ensuring that the applicator can fully extend the gun control arm as far away from the body as possible (usually achieved by providing a spring loaded gun support cable}
Ensuring that the air flow across the face of the booth is adequate to suck the powder away from the operator.
Once these areas are addressed then we can look at adequate PPE:
Hooded disposable overalls.
Gloves (with palm cut outs for gun earth}
Full hood respirator fitted with appropriate cartridges (usually belt mounted fan driven for positive pressure}
Safety boots without rubber (insulating) soles or alternately earthing drag straps.
Hope this helps.
Regards,
Bill
Trainer - Newcastle Australia
Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!