Search for black plating process


1998

We currently use a process called "Electroblack" to produce black deposits on copper,silver,tin,bronze and nickel plated parts for the fashion industry.

We are looking for a replacement for this process that does not contain nickel for the production of nickel-free products. We don't mind cyanide as we have facilities to treat the waste but the process must be free of nickel.

Any suggestions

regards

bob lynch
Bob Lynch
plating company - Sydney, Australia



Hi BOB!
You can use black chrome. It is a very nice finish. We can plate for you some samples.

Arie Porat
furniture mfgr. - Israel
1998



1999

For copper and brass blackening you can use alkaline solutions with oxidizers, for silver you can use sulfide based products, etc. Just make sure that you do not use selenium based products as they are worse than nickel containing products.

Ask your supplier for blackening products, I am sure he will come up with good recommendations.

sara michaeli
sara michaeli signature
Sara Michaeli
Tel-Aviv-Yafo, Israel


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"