finishing.com -- The Home Page of the Finishing Industry Search our quarter-million Q&As

Home of the finishing HOTLINE since 1989

-----

Advise on powder coating wood (for School Project)


1998

I am a team member of a graduate group working on a business plan for Powder Coating on Wood. We are looking for success stories and failures to support our plan. We are also interested in the process. Does the wood have to be preheated, has anyone done any wood other than medium density fiberboard?

The catalyst for this project was a blurb on the front page of the Wall Street Journal stating that Morton had a new powder for wood. Do any of the other powder manufacturers offer a similar product.

Any comments are appreciated.

Jeff N [last name deleted for privacy by Editor]
- Babson College MBA - Massachusetts


Yes, our process demands we preheat the MDF to 250 degrees. Herbert O'Brien and Tiger Drylac have engineered low temperature wood powders for wood. Good luck with your project.

Troy Arie
powder coating - Oklahoma City, Oklahoma
1998



Tons of work have been conducted in the last three to five years. A number of independent labs have toyed with this concept throughout the world.

Kevin Biller
1998



We have had several trials with MDF Board or Supawood as we call it in South Africa. At this stage I am in the process in manufacturing a complete plant for the sole purpose for experimenting a production unit in-house.

Any assistance by means of technical specs would be appreciated. Reciprocal information will be made in return.

Gerald Nagel
- South Africa
2000



Numerous inroads have been made in coating MDF. A preheat is generally required with the product temperature in the range of 200-250 degrees F at application. The post cure can be achieved with gas convection, infrared, or UV curing depending on the specific formulation.

David Koplin
- Freeport, Illinois USA
2001


Yes reheat is one process used.

Powder coating on wood and MDF is in the state with approx. 10 installation using 2 types of powder. Lab and testing work being done in NJ and others across there country. All the major companies have and are developing new powders daily for MDF, Solid and Plywood with great results.

The interesting industries to date are Display, Office Equipment, RTA and Kitchen.

William P Coronato
- Toms River, NJ
2002


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"