Letter 21045

Corrosion and heat treatment  

+++

1. Does Heattreatment [Case hardening] affect corrosion [RUST] properties of steel [SAE J403 1010]?

2. Will the different furnace operating conditions induce different corrosion properties. If yes, what are the conditions that cause.