Clear lacquering brushed stainless steel
+++
We want to clear lacquer our range of brushed stainless steel
domestic radiators. We've tried powder coating but our attempts
weren't scratch resistant enough, any ideas would be most welcome.
Thanks,
Phil Ward
- London, UK