We are having a problem with "White Rus" and discoloration on some
CRS plated parts after the parts are powder coated. The customer
specification for plating is as follows: FINISH: ZINC PLATE PER ASTM
B-633 [link is to info about spec at TechStreet]-85, TYPE II Fe/Zn
8, COLOR YELLOW CHROMATE The parts are then powder coated. What can
we do to prevent this from happening and allow for the maintenance of
the shiny Gold Zinc appearance?
Regards,
Dan Chew
- Round Rock, Texas, USA