Letter 2082

Stripping electrolytic nickel from copper

--

I am hoping to strip electrolytic nickel(sulfamate)from copper without attacking the part. Does anyone have any experience stripping nickel from copper? Typical thickness of 1 mil. I have heard of B-9 strippers from Metalx being effective... Any recommendations would be greatly appreciated.