Letter 2058 Fluoboric Acid based Lead Strip-- We are a small plating and metal cleaning facility in central Tx. We are searching for a "RECIPE" to strip lead using Fluoboric Acid. The product that we are currently using is extremely effective but costly. Any information at all would be greatly appreciated. Thank you, Kitt Daly GTI Coatings, Inc. - Austin, TX.
. We also have an interest in a lead stripping process. Did you have any responce to the request for a fluoboric Acid formula? Ron Rowley