Dear Sir,

We have a problem of testing the adhesion of the electroplated Ni layer. We would like to use a non-destructive testing method to test the adhesion strength of the coating.
The available destructive testing method, pull-off testing was suggested for this electroplated layer. But the polymer bonding between the electroplating and the testing assembly is not good compared to the adhesion of the electroplating and the substrate. So it is difficult to test the same using this.
Please suggest some ideas to test the same

Yours Truly,

Rajagopalan Ramaseshan
Kawasaki Heavy Industries Ltd


.

Mr. Rajgopalan, I do not know a non-destructive test for nickel adhesion, but the simple destructive test is soldering a plug or a wire to nickel for pull testing.

Mandar Sunthankar
- Fort Collins, CO


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com