Letter 2039

--

We are starting with a small hot dip galvanizing plant we are having the following problems.

Big deformation on pieces (14 gauge bucket for fish)
Wera nor getting uniform deposition
What tips will you suggest to try

Thanks

Felix Rossel Enatin - Guyaquil Ecuador