Home of the finishing HOTLINE since 1989

-----

What is the composition of Inconel


Q. Could someone please provide me with a breakdown of materials in Inconel? (Including percentages of each).I am told that it contains: nickel, chrome, columbium and titanium. Is this correct and are there any other constituents? Any help would be greatly appreciated.

Jeff Mills
metal finishing shop - Gorham, Maine
1998


A. Inconel is 14 percent Cr, 6 percent Fe, balance Ni. See the Electroplating Engineering Handbook ⇦ this on eBay, AbeBooks, or Amazon [affil link] for more info

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.




Q. I seem to remember at college, being told that the name "Inconel" was actual made up from some abbreviations, possibly of metals. Does anybody know where the name "Inconel" actually came from?
Thanks,

colin parsons
- Saudi Arabia
1999


A. INCONEL--THIS IS A TRADE NAME OF INTERNATIONAL NICKEL. I HAVE MOST OF THEIR LITERATURE AND WILL ANSWER ANY QUESTIONS TO DO WITH NICKEL ALLOYS AND STAINLESS STEEL.

ROBERT RIDDOCH
- MONTREAL, QC, CANADA
2002


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"