Zinc Plating Appearance Problems


We are seeking a means of coating parts that is more consistent than the finish we have been getting by specifying Zinc plating on steel and Anodized finishes on aluminum. We currently refer to the ASTM specs on our drawing but that has not assured us of consistent appearance.

Jim Crowley
- Lehigh Valley Pennsylvania
1998



Dear Jim ,

You & only you know the areas of use of your product therefore it is best that you use the ASTM specifications as a guide only and produce your own specifications based upon them .

Be demanding & very specific in what you want , need more advice employ an experienced consultant to prepare the specifications for you.

Regards

John Tenison-Woods
John Tenison - Woods
- Victoria Australia
1998


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"