Letter 20060

How to obtain deeper well aligned porous titanium dioxide? [China] 

+++

I have obtained well aligned porous titanium dioxide by using anodizing technique, but only about 300 nm depth, how to get deeper ones, for about several micrometers?

Qunliang Song
- Shanghai, P.R.China

Ed. note: please explain whether you used alkaline or acid anodizing, and what electrolyte and voltage you used. Thanks! Anodizing is a self-limiting process because the anodized film is a resistor that stops permitting passage of current at a given voltage after a certain thickness has been obtained.


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
I want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     