Letter #20000

Nikasil treatment - what is involved in the process [South Africa] 

+++

Having searched for many hours trying to find more information about the nikasil treating process we would like to know how exactly it is done and what equipment is needed to carry out the whole process. Any useful information would be appreciated.

Thanks,

Kyle C.
a bicycle manufacturer - Ixopo, Natal South Africa


++++

Hello, Mr. Cutler. Nikasil is a trademark, and you would need to contact the manufacturer if you wished to buy or license the process. But my understanding is that it is nickel silicon carbide plating and that competitive processes are available from other companies.

 
Ted Mooney, P.E.
finishing.com Inc. - Brick, NJ